TAPPI TIP 0304-37
- Comments Off on TAPPI TIP 0304-37
- TAPPI
Click here to purchase
The corrugated industry has moved toward higher usage levels of recycled liner and denser liners to meetcustomer requirements and to help the environment. These changes require plants to control their normal operatingpractices on the corrugator as well as in the press department to avoid score cracking problems.
All liners can crack or check under hot or dry atmospheric conditions, and even in cool moist atmosphericconditions, if the liners have been over heated on the corrugator. The cracking problems occur most frequently at thescore lines. Cracking is especially evident during the drier winter months, or in heated storage environments. Today,many corrugated operations are modifying their machines to run hotter and faster, thus further increasing incidents ofcracking.
The retention of moisture in combined board is a very important element to successfully score corrugated board.Most plants are now checking their combined board’s total moisture content, measuring it off of the dry end of thecorrugator with an automatic weighing and drying oven (see Special Note). Experience has demonstrated that a targetmoisture from 5.8 to 7.5% total combined board moisture works well throughout the year. Corrugator operatingtechniques will need to be under control if liners are to be run without quality problems.
Maintenance of the press, especially in regards to Total Indicated Run out (TIR) and axial head movement in anyarea that applies pressure to the combined board, is critical for preventing score cracking.
This Technical Information Paper (TIP) includes recommended operating procedures to minimize incidents ofscore cracking.
Product Details
- Published:
- 06/01/2023
- Number of Pages:
- 4