SAE J815_201211
- Comments Off on SAE J815_201211
- SAE
Click here to purchase
Traditionally, cellular foam products have been checked for load deflection by determining the load required to effect a 25% deflection. In automotive seating, on the other hand, the load deflection checked by determining the thickness under constant force conditions to (a) indicate the initial softness of the seat cushion, (b) measure how thick the seat cushion is under average passenger load (a measurement of padding left for “ride” and seated height), and (c) determine a value to indicate resiliency. In this method these measurements are made by determining the thickness of the seat cushiong under fixed loads of 4.5 N, 110 N, and 220 N with a 323 cm\u2 circular indentor foot.
Product Details
- Published:
- 11/19/2012
- File Size:
- 1 file , 160 KB