IEC 60317-50 Ed. 2.0 b:2012
- Comments Off on IEC 60317-50 Ed. 2.0 b:2012
- IEC
Click here to purchase
IEC 60317-50:2012 specifies the requirements of glass-fibre wound resin or varnish impregnated, bare, grade 1 or grade 2 enamelled round copper winding wire, temperature index 200. The impregnating agent is silicone resin based. For this type of wire, the heat shock test is inappropriate and therefore a heat shock temperature cannot be established. Consequently, a class based on the requirements for temperature index and heat shock temperature cannot be specified. This edition includes the following significant technical changes with respect to the previous edition:
– addition of requirements for appearance, new subclause 3.3 and
– addition of pin hole test requirements, Clause 23: Pin hole test. Keywords: copper winding wire
This publication is to be read in conjunction withIEC 60317-0-6:2001.
Product Details
- Edition:
- 2.0
- Published:
- 07/09/2012
- Number of Pages:
- 20
- File Size:
- 1 file , 200 KB